| 讯号 | 项目 | 100 | 150 | 200 | 250 | 300 | 350 | 400 | 450 | 500 | 600 | 800 | 备注 |
| 1 | 单位面积质量偏差% | -8 | -8 | -8 | -8 | -5 | -7 | -7 | -7 | -6 | -6 | -6 | |
| 2 | 厚度,mm≧ | 0.9 | 1.3 | 1.7 | 2.1 | 2.4 | 2.7 | 3.0 | 3.3 | 3.6 | 4.1 | 5.0 | |
| 3 | 幅宽偏差% | -0.5 | |||||||||||
| 4 | 断裂强力KN/M≧ | 2.5 | 4.5 | 6.5 | 8.0 | 9.5 | 11.0 | 12.5 | 14.0 | 16.0 | 19.0 | 25.0 | 纵横向 |
| 5 | 断裂伸长率% | 25-100 | |||||||||||
| 6 | CBR顶破强力KN≧ | 0.3 | 0.6 | 0.9 | 1.2 | 1.5 | 1.8 | 2.1 | 2.4 | 2.7 | 3.2 | 4.0 | |
| 7 | 等效孔径O90mm | 0.07-0.2 | |||||||||||
| 8 | 垂直渗透系数cm/s | KX(10-1-10-3) | K=1.0-9.9 | ||||||||||
| 9 | 撕破强力KN | 0.08 | 0.12 | 0.24 | 0.24 | 0.24 | 0.28 | 0.33 | 0.38 | 0.42 | 0.46 | 0.6 | |